# Bell Alert Service Bulletin 205-13-109

Copy: No revision named ("U.S. DOT/FAA - Bell ASB No. 205-13-109 IR Dated 2-04-13 - TR Blades.png"), 4 pages: PDF https://openairdocs.org/files/sha256/28/d5/28d5d9e50f03cb8620d6d0899f9138e2afc30d60adf509fd46f30bb5033988f4; text https://openairdocs.org/service-documents/bell/sb-205-13-109/file/28d5d9e50f03.md. Rights: © Bell Textron Inc. Filed by the FAA in regulations.gov docket FAA-2013-0639; AD 2013-15-02 incorporates this document by reference. Not covered by OpenAirDocs’ CC0 dedication.

## Details

- Manufacturer: [Bell](https://openairdocs.org/service-documents/bell.md)
- Type: Service bulletin (Alert Service Bulletin)
- Number: 205-13-109
- Page: https://openairdocs.org/service-documents/bell/sb-205-13-109

## ADs that cite it (1) (OpenAirDocs)

Newest first, with the revision each names, as OpenAirDocs read it from the AD's text.

- [AD 2013-15-02](https://openairdocs.org/ad/2013-15-02.md), effective Aug 14, 2013: No revision named

## Text (4 pages)

Rights: © Bell Textron Inc. Filed by the FAA in regulations.gov docket FAA-2013-0639; AD 2013-15-02 incorporates this document by reference. Not covered by OpenAirDocs’ CC0 dedication. Each page's text from the PDF; open the PDF at a page with #page=N.

### Page 1

ASB 205-13-109 
Page 1 of 4 
ECCN EAR99 
 
 
 
 
 
  ALERT SERVICE BULLETIN 205-13-109 
4 February 2013 
 
 
 
MODEL AFFECTED:  205A/205A-1 
 
SUBJECT: TAIL ROTOR BL ADE P/N 212-010-750-ALL, 
INSPECTION OF 
 
HELICOPTERS AFFECTED: Seri al number 30001 through 30332. 
 
  
COMPLIANCE: Within the next 25 hours and every 25 hours 
thereafter 
 
 
DESCRIPTION: 
 
Bell Helicopter has recently examined a fractured tail rotor blade; the fracture 
originated from surface damage. This ASB introduces a 3X magnifying glass 
inspection of the tail rotor blade surface for damage every 25 hours. Any damage is to 
be investigated by removing paint an d inspecting skin condition with 10X 
magnification.  Due to the crit ical nature of this inspection and requirements to fully 
comply, Bell Helicopter is adding a local in spection with 10X magn ification of blade 
between stations 20.00 to 35.00  from the leading edge to t he trailing edge. This is in 
addition to the 3X requirement  for the full blade. Operator s are reminded that it is 
critical to investigate any paint and skin imperfections should the inspection warrant. If 
anomalies are noted during the 3X/10X inspec tions of the blade surface, remove the 
paint and check skin condition again with 10X magnification. Skin damage exceeding 
Maintenance Manual limits requires blade remova l from service. Applicability of this 
bulletin to any spare part sha ll be determined prior to its in stallation on an affected 
helicopter. 
 
APPROVAL: 
 
The engineering design aspects of this bulletin are FAA/ODA approved.

### Page 2

ASB 205-13-109 
Page 2 of 4 
ECCN EAR99 
CONTACT INFO: 
 
For any questions regarding this bulletin, please contact: 
 
Bell Helicopter Product Support Engineering - Medium Helicopters 
Tel: 450-437-6201 / 1-800-363-8028 / psemedium@bh.com 
 
MANPOWER: 
 
Approximately 1.0 man-hour is required to complete this bul letin.  This estimate is 
based on hands-on time, and may vary with personnel and facilities available. 
 
WARRANTY: 
 
There is no warranty credit applicable for parts or labor associated with this bulletin. 
 
MATERIAL: 
 
Required Material: 
 
The following material may be required for the accomplishment of this bulletin and 
may be obtained through your Bell Helicopter Textron Supply Center. 
 
Part Number Nomenclature  Qty   
    
212-010-750-133 Bl ade  A/R  
 
Consumable Material: 
 
The following material may be required to accomplish this bulletin, but may not require 
ordering, depending on the operator’s consumable material stock levels.  This material 
may be obtained through your Bell Helicopter Textron Supply Center. 
 
Part Number Nomenclature  Qty  Reference * 
    
P-C-451 Abrasive Cloth or Paper, 
Aluminum Oxide 
A/R C-406 
 
* C-XXX numbers refer to the consumables list in BHT-ALL-SPM Standard Practices Manual 
 
SPECIAL TOOLS: 
 
None required.

### Page 3

ASB 205-13-109 
Page 3 of 4 
ECCN EAR99 
WEIGHT AND BALANCE: 
 
Not affected. 
 
ELECTRICAL LOAD DATA: 
 
Not affected. 
 
REFERENCES: 
 
BHT-205A1-IPB Illustrated Parts Breakdown 
BHT-205A1-MM Maintenance Manual 
BHT-205A1-CR&O Component Repair and Overhaul Manual 
 
PUBLICATIONS AFFECTED: 
 
BHT-205A1-MM Maintenance Manual. 
 
ACCOMPLISHMENT INSTRUCTIONS: 
 
1. Prepare helicopter  for maintenance. 
-NOTE- 
 
Removal of the tail rotor blades is not required for this 
inspection. 
 
2. Clean each tail rotor blade by hand us ing mild soap and cheesec loth (C-486) in a 
spanwise direction.  Dry thoroughly. 
3. Carry out a detailed visual  inspection of both sides of the entire blade with a 3X 
magnifying glass and a bright light. Ins pect the tail rotor blade skin, leading edge 
spar, doublers, grip plates and trailing edge  for cracks, corrosion, nicks, dents and 
scratches. Refer to Maintenance Manual for damage limits. 
4. Carry out a further detailed visual ins pection with 10X magnifi cation of the shaded 
area shown in Figure 1 between stations 20 .00 to 35.00 of both sides of the blade 
with a bright light. 
5. If any blistering, peeling, flaking, bubbling or cracked paint is detected, remove the 
paint from the affected area by s anding in a spanwise direction only  with an 
abrasive cloth or paper (C -406) 240 grit or finer and a final sanding using an 
abrasive cloth or paper (C- 406) 400-grit or finer. After paint removal, visually 
inspect the affected area for damage us ing a 10X magnifying glass.  Damage 
beyond the limits of the Maintenance Manual requires blade removal from service.

### Page 4

ASB 205-13-109 
Page 4 of 4 
ECCN EAR99 
6. Only superficial corrosion that can be re moved with aluminum wo ol or very fine 
grade abrasive pad (C-407) is permissible.  Corrosion on the spar 0.003 inch deep 
or less is acceptable when polished out. Replace any blade that has corrosion on 
the spar greater than 0.003 inch. 
7. If a nick, scratch or dent is found, visu ally inspect for crack using a 10X magnifying 
glass or higher, and measure the dept h of the damage. (A digital optical 
micrometer is one tool that can be used for this measurement). 
8. Repair damage and/or co rrosion found on tail rotor bl ades in accordance with the 
Maintenance Manual. 
9. Replace any blade that has a cr ack. No cracks are permitted. 
10. If paint was removed during the above steps, carry out paint touch up/refinishing as 
per BHT-205A1-CR&O, Chapter 65. 
11. Make an entry in the helicopter logbook a nd historical service record to indicate 
accomplishment of this ASB. Enter exact lo cation of blend repair (if applicable) in 
the historical service record. Location shall include blade station as well as 
distance from the leading edge. 
 
 
 
 
 
 
Figure 1

---
OpenAirDocs.org is an independent research project of [Contrail Labs](https://contraillabs.com/). It is not affiliated with the FAA or the NTSB. Source documents are U.S. government works in the public domain, except the copies of manufacturers’ service documents, which belong to their rights holders.