JASC 5310
Service difficulty reports · 38,573
Reports filed under 5310 · Fuselage Main, Structure, newest first.
Query with SQL
duckdb -csv -c "SELECT sdr_id, difficulty_date, n_number, aircraft_make, aircraft_model, part_name, part_condition, jasc_code, discrepancy FROM 'https://openairdocs.org/data/latest/faa_service_difficulty_report.parquet' WHERE jasc_code = '5310' ORDER BY difficulty_date DESC"
Prints the whole list as CSV. It reads the release’s Parquet files over HTTPS, so there’s nothing to download first. Install DuckDB to run it.
SELECT sdr_id, difficulty_date, n_number, aircraft_make, aircraft_model, part_name, part_condition, jasc_code, discrepancy FROM 'https://openairdocs.org/data/latest/faa_service_difficulty_report.parquet' WHERE jasc_code = '5310' ORDER BY difficulty_date DESC
Run it at the DuckDB prompt, or in any tool that reads Parquet over HTTPS. More ways to query the release are on Use the data.
SDR AALA20000578Shear Tie · crackedTUL - FOUND CRACK IN SHEAR TIE BETWEEN L613 AND L614 STATION 1380. STOP DRILLED CRACK. INSTALLED DOUBLER PER AARD 53-10-00-20. (M)SDR QXEA0001043Structure · tornPDX - RT NOSE LANDING GEAR BAY INNER STRUCTURE TORN AND DENTED AT FORWARD LOWER WEB, APPROXIMATELY STATION 2650. REPAIRED IAW FOKKER SRM 53-01-01, PAGE 8, PARAGRAPH 5C AND SRM 51-10-4.SDR RRXA001696Structure · crackedDURING A MAINTENANCE VISIT, FOUND A CRACK BEHIND LT NOSE LANDING GEAR DOOR ON FUSELAGE, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. STOP DRILLED CRACK, FABRICATED DOUBLER FROM 7075-T6 AND INSTALSDR P2EA00082Housing · damagedYXD - DURING C-CHECK, FOUND REPAIR PLATE ON BELLCRANK HOUSING COMPLETELY SEVERED BS 680, BL 28L WL 208.1. REPLACED REPAIR PLATE ON BELL CRANK HOUSING BS 680, BL 28L, WL 208.1 PER SRM 51-10-1, 51-10-3 WORK ACCOMPLISHED ON NON-ROUTINE NR 0404. (M)SDR 0001562275Strap · corrodedDURING H CHECK, FOUND CORROSION ON BEAR STRAP AT NR 2 MAIN CARGO DOOR. REPAIRED PER EA22-175139.SDR 00FDEA00179Stringer · corrodedCORROSION (C53-224-01, 2) CORROSION ON STRINGER 8 LT AT BS 783 TO 825. *S/D* ALODINED, PAINTED AND REPAIR PARTS PER IAW FEDEX 51-20-151, 51-30-2 & 53-10-3.SDR ASAA0080220Beam · corrodedPHX - DURING 30K CHECK, THE AFT CARGO COMPARTMENT DOOR BEAM AT FS 1173, LONGERON 29R WAS FOUND CORRODED. REMOVED CORROSION AND REPAIRED PER SRM 51-30. (M)SDR AU000399Post · cracked(AUS) LT COCKPIT C-D WINDOW POST CRACKED. CRACK LENGTH 6.35MM (0.25IN). FOUND DURING INSPECTION IAW ER B73-53-10-6 (AD/B737/12).SDR RRXA001942Structure · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE AFT LWR CARGO BILGE STA 1260 TO 1280 AND L34R, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. RECEIVED REPAIR AND INSTALLED IAW DC-8 SRM 53-2-0 ASDR F3LA00062Structure · brokenDEN - DURING C-7 CHECK INSPECTION, REPORTED EXPANSION JOINT FORWARD OF CENTER FUEL TANK, LEFT OF CENTER LINE, BROKEN. MAINTENANCE REPLACED CHANNEL ASSY PER SRM 53-21-00. (M)SDR USAA000431Door Frame · crackedCLT - DOOR FRAME CRACKED .5 INCH, FORWARD SERVICE DOOR FRAME, LOWER FORWARD CORNER. INSTALLED DOUBLER AND FILLER PER SRM 51-40-04. (M)SDR RRXA002155Door Frame · crackedDURING A MAINTENANCE VISIT FOUND A CRACK TO THE MAIN CARGO DOOR LOWER AFT CORNER FRAME, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED REPAIR AND INSTALLED IAW 53-2-3.SDR RRXA002154Door Frame · crackedDURING A MAINTENANCE VISIT FOUND A CRACK TO THE MAIN CARGO DOOR UPPER AFT CORNER FRAME, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED REPAIR AND INSTALLED IAW 53-2-3.SDR USAA000370Angle · crackedCLT - FOUND ANGLE CRACKED 2 INCHES, LEFT HORIZ STAB CUTOUT S5A. INSTALLED REPAIR ANGLE PER SRM 53-00-01 FIG 221 AND EA 66811. (M)SDR AALA20000581Shear Tie · crackedTUL - FOUND SHEAR TIE CRACKED FORWARD SIDE OF STATION 1309 FRAME BETWEEN LONGERON 14R AND 15R. REMOVED AND REPLACED SHEAR TIE PER SRM 51-01. (M)SDR AALA2000525Structure · crackedTUL - FOUND RBL 8 VERTICAL CRACKED AT LOWER END, PER SB 727-53-0175 REV 3. (M)SDR AU000137Structure · fractured(AUS) NOSE LANDING GEAR NACELLE STRUCTURE FAILED IN THE AREA OF THE UPPER ACTUATOR ATTACHMENT POINT. NLG COLLAPSED DURING LANDING CAUSING DAMAGE TO THE SURROUNDING STRUCTURE AND BOTH PROPELLERS. SUSPECT STRUCTURE HAD BEEN DAMAGED FOR SOME TIME BEFORE FINAL FSDR MWEA00168Frame · damagedTOOLING DAMAGE ON FRAME 661 AT LONGERON 17R, 16R, AND 15R. FABRICATED AND INSTALLED NEW FRAME SECTION AND REPAIR SPLICES.SDR RRXA000712Web · crackedDURING A MAINTENANCE VISIT FOUND A CRACK ON THE WEB AT STA 1160 LONGERON 33R, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. /////CORRECTIVE ACTION///// REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED REPAIRED DOUBLER AND FILLER IAW SDR P2EA00094Door Frame · crackedYXD - DURING C-CHECK, FOUND R-1 DOOR FRAME INTERCOSTAL AT BS 332 STRINGER 11 CRACKED, LENGTH .500 INCH. REPAIRED R-1 DOOR INTERCOSTAL AT BS 332, STRINGER 11 WITH DOUBLER PER SRM 51-40-3 FIG 1 WORK ACCOMPLISHED ON NON-ROUTINE NR 137. (M)SDR UIEA01012Shear Tie · crackedDURING ROUTINE INSPECTION, FOUN FRAME SHEAR TIE CRACKED IN RADIUS BETWEEN STATION 340-360 R/S AT MAIN DECK LEVEL (WBL200). TRIMMED DAMAGE AREA. MANUFACTURED REPAIR ANGLES AND FILLER. INSTALLED PER STANDARD PRACTICES WITH RIVETS BACR15BB5AD. (M)SDR RRXA000697Intercostal · damagedDURING A MAINTENANCE VISIT FOUND A HOLE IN INTERCOSTAL IN THE RADIUS OF TOP FLANGE STA 89 AND LBL 18, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED DOUBLER IAW DC-8 SRM 53-2-0 FIG 1B, 51-SDR USAA000319Frame · crackedCLT - FOUND FRAME CRACKED .125 INCH, STATION 867 BETWEEN STRINGER 8L AND STRINGER 9L. INSTALLED FILLER AND DOUBLER PER TR 53-10-14. (M)SDR 0000719621Skin · corrodedCABIN WINDOW FRAME NR 20 RT HAS CORROSION ON AFT INNER SKIN SURFACCE OF WINDOW OPENING. REF EA 96-172247 LOG PAGE 1405947.SDR RRXA000680Gusset · missingDURING A MAINTENANCE VISIT FOUND A GUSSET MISSING AT THE INTERCOSTAL AT STA 1660 LONGERON 4L, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. /////CORRECTIVE ACTION///// REMOVED DAMAGE, TREATED, ALODINE AND PRIMED AREA IAW DC-8 SRM 51-1-8. FABRICATED GUSSET AND SDR ASAA0080177Shear Tie · corrodedPHX - DURING 15K CHECK, THE MID CARGO COMPARTMENT MAIN FRAME SHEAR TIE CLIP WAS FOUND CORRODED AT FS 636, LONGERON 29R-30. REPAIRED PER SRM 51-30-5. (M)SDR RRXA003410Shear Tie · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE SHEAR TIE AT FS 55 AND BETWEEN L35L TO L34R, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED PART IAW DC-8 SRM 51-1-21 AND DWG 56138SDR RRXA003000Shear Tie · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE SHEAR TIE AT FS 35 AND L35L TO L34R, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED REPAIR AND INSTALLED IAW DC-8 SRM 51-1-21 AND DWG. #5613836SDR RRXA000720Intercostal · crackedDURING A MAINTENANCE VISIT FOUND A CRACK TO THE INTERCOSTAL BOLT AT STA 240 TO 260 LONGERON 11R, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. /////CORRECTIVE ACTION///// REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED IAW SDR RRXA000919Door Frame · crackedDURING A MAINTENANCE VISIT, FOUND A CRACK TO THE FUSELAGE STRUCTURE AT AFT FRAME JAMB (R2 DOOR) AT STA 1500 R, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. FABRICATED DOUBLER FROM 2024-T3 AND INSTASDR RRXA000544Shear Tie · corrodedDURING A MAINTENANCE VISIT, FOUND CORROSION DAMAGE TO SHEAR TIE AT STA 35, AND IN BETWEEN LONGERON 35 LEFT TO 34 RIGHT, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED SHEAR TIE IAW DC-8 SRSDR AALA2000432Structure · crackedTUL - FOUND CRACK EMANATING FROM FASTENER IN W/W STATION 870 BELOW LOAD CONTROL VALVE. REMOVED AND REPLACED CRACKED VERTICAL STIFFENER AS PER ESO 11697 DATED 2/23/2000. (M)SDR RRXA003796Sill · damagedDURING A MAINTENANCE VISIT FOUND MISSING NUT PLATE TO B-PIT DOOR LWR SILL HOLES, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. WELDED BAMAGE AND INSTALLED NUT PLATES IAW E.O. 00-016 WITH APPROVED 8110-3 DATED 02/18SDR ASAA0080505Shear Tie · corrodedPHX - DURING SCHEDULED 30K CHECK, THE AFT CARGO COMPARTMENT STATION 1287 BETWEEN LONGERON 29L TO 30L SHEAR TIE WAS FOUND TO BE CORRODED. REPAIRED PER SRM. (M)SDR AU000162Door Frame · cracked(AUS) CARGO DOOR OUTER FRAME CRACKED IN FIVE PLACES ON THE LOWERFORWARD CORNER. FOUND DURING EDDY CURRENT INSPECTION.SDR RRXA000717Door Frame · crackedDURING A MAINTENANCE VISIT FOUND A CRACK TO THE NUT PLATE MOUNTING POINT ON A-PIT DOOR FRAME (AFT SIDE) AT STA 340, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. RECEIVED AND INSTALLED NEW SUPPORT FRAME IAW DC-8 SDR AU000209Structure · damaged(AUS) RIGHT FORWARD WING ATTACHMENT FITTING TO FUSELAGE UNDER TENSION. THE FUSELAGE IN THIS AREA BULGING AND CRACKING. INTERNAL STRESS DAMAGE AND CRACKING. CAUSE OF DAMAGE UNKNOWN.SDR AU000263Structure · damaged(AUS) FUSELAGE SKIN CRACKED IN AREA OF LEFT WING FORWARD ATTACHMENT FITTING. INTERNAL STRUCTURE ALSO DAMAGED IN THE SAME AREA. CENTER SECTION LOWER FUSELAGE FRAMES BUCKLED AND LOWER SKIN DAMAGED.SDR AALA2000331Structure · corrodedTUL - FOUND CORROSION AROUND FASTENER HOLE .017 MATERIAL REMOVED. REPAIRED PER ESO 30595, DATED 2/16/200 AND SRM. (M)SDR RRXA000941Structure · crackedDURING A MAINTENANCE VISIT, FOUND 5 CRACKS TO THE BULKHEAD THRU DOOR AT THE AFT LOWER CARGO BILGE AT STA 1380, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. RECEIVED AND INSTALLED NEW BULKHEAD DOOR IAW DSDR RRXA003788Threshold · crackedDURING A MAINTENANCE VISIT FOUND CRACK DAMAGE TO CABIN R1 DOOR TRESHOLD AFT I/B CORNER AT STA. 190, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. WELDED CRACKED SECTION, NDT INSP PER ASTM E1417, NO DEFECTS NOTED. ISDR AU000145Structure · corroded(AUS) LEVEL 2 CORROSION FOUND AS A RESULT OF AD/B737/52 AMDT6.SDR AU000144Structure · corroded(AUS) LEVEL 2 CORROSION FOUND AS A RESULT OF AD/B737/52 AMDT6.SDR TWAA0003013Structure · damagedDURING OP 16 MAINT CHECK, NECESSARY TO REPAIR HOLE DAMAGE IN FUSELAGE AT APPORX STA 608 TO 612, LONGERON 28L TO 28R. COMPLIED WITH ARA 16532.SDR ASAA0080110Shear Tie · corrodedPHX - DURING 15K CHECK, FOUND CORROSION ON THE AFT CARGO COMPARTMENT FORWARD SIDE OF FRAME AT SHEAR TIE, STATION 1174, LONGERON 29R TO 30. REMOVED CORROSION PER SRM 53-01. (M)SDR DL72L000285Noise · detectedDURING CLIMBOUT A INTERMITTENT THUMPING NOISE WAS HEARD WHICH APPEARED TO BE COMING FROM UNDER THE 1ST CLASS CABIN. THUMPING CONTINUED AT CRUISE FL330 FOR ABOUT 15 MIN AND THEN QUIT. INSPECTED E&E, FWD CARGO PIT, FWD DOORS INCLUDING E&E, L1, L2, F/CARGO DOORSDR 20000831SH009Forging · corrodedWINDOW FORGINGS CORRODED BS 540 - BS 560 RIGHT SIDE, BS''S 1140-1160 RIGHT SIDE, 1200 - 1220 RIGHT SIDE, 600J - 620 LEFT SIDE AND 800 - 820 LEFT SIDE. (X)SDR RRXA003789Skin · crackedDURING A MAINTENANCE VISIT FOUND CRACK DAMAGE TO CABIN R-1 THRESHOLD FWD I/B AT STA. 170, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. WELDED CRACK IAW MIL-STD 2219, NDT C/W IAW ASTM E 1417, NO FLAWS NOTED. INSTALSDR RRXA002966Structure · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE SIDEWALL TUNNEL AT STA 1100 AND L24L - L26L, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED REPAIR IAW DC-8 SRM 51-1-20D. (CORROSISDR USAA000138Frame · crackedCLT - FOUND FRAME CRACKED .5 INCH, BS 747 BETWEEN STRINGER 8R AND 9R. INSTALLED FILLER AND DOUBLER PER TR 53-10-14. (M)
Back to JASC 5310