Boeing 727-25C
Service difficulty reports · 2,007
Newest first. General aviation reporting is voluntary.
Query with SQL
duckdb -csv -c "SELECT sdr_id, difficulty_date, n_number, aircraft_make, aircraft_model, part_name, part_condition, jasc_code, discrepancy FROM 'https://openairdocs.org/data/latest/faa_service_difficulty_report.parquet' WHERE aircraft_model_key = '72725C' ORDER BY difficulty_date DESC"
Prints the whole list as CSV. It reads the release’s Parquet files over HTTPS, so there’s nothing to download first. Install DuckDB to run it.
SELECT sdr_id, difficulty_date, n_number, aircraft_make, aircraft_model, part_name, part_condition, jasc_code, discrepancy FROM 'https://openairdocs.org/data/latest/faa_service_difficulty_report.parquet' WHERE aircraft_model_key = '72725C' ORDER BY difficulty_date DESC
Run it at the DuckDB prompt, or in any tool that reads Parquet over HTTPS. More ways to query the release are on Use the data.
SDR UPS99231226Seat Track · corrodedINSPECTION TYPE:SI, MAIN DECK SEAT TRACK HAS CORROSION ON TOP OF TRACK, BS 760 AND BS 780 RBL 63 WL 208. REMOVED CORRODED SEAT TRACK, FABRICATED AND INSTALLED NEW SEAT TRACK PER SRM 53-10-1, SRM 51-30-5, SRM 51-10-2 AND SRM 51-30-2.SDR UPS99231225Stringer · corrodedINSPECTION TYPE:SI, CORROSION (C53-224-01.00-01) MAIN DECK LONGITUDINAL BEAM BS 760-848 LBL 45 WL 208 RT FLANGE SEVERAL PLACES. REPAIRED PER SRM 51-10-2, 51-30-2.SDR UPS99231214Sill · corrodedINSPECTION TYPE:SI, CORROSION (C53-224-01.00-01) ON MOP SILL ANGLE BS 312 BS 344 LBL 58 WL 208. REMOVED, REPLACED MOP SILL PER SRM 51-30-2, 53-10-1.SDR UPS00231405Frame · corrodedINSPECTION TYPE:SI WHILE ACCESSING MCD FOR NDT, FOUND CORROSION UNDER SEAL DEPRESSOR BS 620 LT ABOVE SPLICE WL 268 ON FRAME. REPAIRED CORRODED FRAME IAW ER-6435A.SDR UPS99231167Skin · corrodedINSPECTION TYPE:SI BULGING SKIN AT BS 355, STR 27R, WL 156. REPAIRED BULGING SKIN AT BS 355, STR 27R, WL 156 IAW ER 99-6374 AND SRM 53-30-03 FIG 3A AND ER 99-6412.SDR UPS99231166Shear Tie · corrodedINSPECTION TYPE:SI SHEAR TIE AT BS 480 STR 20-21 RT IS CRACKED AND CORRODED. FABRICATED AND REPLACE SHEAR TIE PER SRM 53-10-4 AND SRM 51-30-2.SDR UPS99231165Stringer · corrodedINSPECTION TYPE:SI CORROSION ON STRINGER AT BS 463 STR 21R. REPAIRED STRINGER PER SRM 53-10-3 FIG 1.SDR UPS99231125Stringer · corrodedINSPECTION TYPE:SI CORROSION ON STRINGER BS 360 TO 380, STR 26L. REMOVED AND REPLACED STRINGER SEGMENT PER SRM 53-10-3 FIG 1.SDR UPS99231136Angles · corrosionINSPECTION TYPE:SI CORROSION (C53-111-01.03-02) ON FWD CARGO BAY CEILING BEAM AROUND 2 EACH FASTENER HOLES BS 580-BS 600, BL 0, WL 200. REMOVED DAMAGE AND REPAIRED PER ERO 99-6278.SDR UPS99231135Beam · crackINSPECTION TYPE:SI CRACK IN VERTICAL BEAM AT BS 1183, LB 18.5, WL 275. REMOVED DAMAGE AND REPAIRED PER UPS EO B727-5310-7267 APPX B.SDR UPS99231132Stiffner · corrodedINSPECTION TYPE:SI CORROSION (C53-111-01.00-01) ON SIDES OF E/E DOOR WARNING SWITCH COVER HOUSING. REPLACED STIFFENER BS 450-452 LBL 10 TO RBL 13 AND DOOR SWITCH HOUSING SAME BS LBL 2 TO RBL 6 PER 727 SRM 51-30-2, 51-20-1, 51-30-5, 51-20-151 AMD MM 52-40-11.SDR UPS99231131Fitting · corrodedINSPECTION TYPE:SI WHILE WORKING TASK CARD NR 1249 FOUND THE NR 4 FLAP TRACK FITTING THAT ATTACHES TO FWD LANDING GEAR TRUNION BEARING TO BE CORRODED. REPLACED FITTING PER SRM 51-30-4.SDR UPS99231130Stringer · corrosionINSPECTION TYPE:SI CORROSION (C53-111-01.00-01) ON STRINGER AT BS 360 TO BS 400 STR 27L. REMOVED CORRODED SECTION AND REPLACED PER SRM.SDR UPS99231129L-Angle · corrosionINSPECTION TYPE:SI CORROSION (C53-221-01.00-01) CORROSION ON FLOOR STRUCTURE L-ANGLE AND WEB AT STA 298 RBL 13, WL 208. REMOVED DAMAGED AND REPAIRED PER SRM.SDR UPS99231128Angle · corrosionINSPECTION TYPE:SI CORROSION (C53-221-01.00-01) CORROSION ON AFT EDGE OF L-ANGLE AT BS 297, RBL 12-RBL 54, WL 208. REMOVED L-ANGLE AND REPLACED.SDR UPS99231127Support · corrosionINSPECTION TYPE:SI CORROSION (C53-111-01.00-02) ON SIDEWALL/BULKHEAD SUPPORT AT BS 680 LBL 31-45 WL 159-166. REMOVED SUPPORT AND REPLACED PER SRM.SDR UPS99231126Aileron · delaminatedINSPECTION TYPE:SI LT O/B AILERON T/E WEDGE IS DELAMINATED AND SATURATED WITH OIL ON THE O/B AFT END. REMOVED A 1 HALF INCH AREA OF DELAMINATED SKIN AT O/B AFT CORNER UPPER AND LOWER SURFACES AND REMOVED CONTAMINATED POTTING COMPOUND. FABRICATED REPAIR PLUGSSDR UPS99231114Stringer · corrodedINSPECTION TYPE:SI, CORROSION ON STRINGER SPLICE AT BS 445, STR 20R. DAMAGE BEYOND LIMITS. REMOVED AND REPLACED STRINGER SPLICE PER BAC DWG 65-18215.SDR UPS99231113Channel · corrodedINSPECTION TYPE:SI, CORROSION (C53-221-01.01-01) ON FLOOR STRUCTURE AT BS 236 WL 208, LBL 32. REMOVED DAMAGE AND REPLACED PER SRM.SDR UPS99231112Skin · corrosionINSPECTION TYPE:SI CORROSION (C53-100-01.07-04) BULGING SKIN AND ONE SHEARED RIVET BELOW THE FORWARD LAV SERVICE PANEL BS 295 TO BS 312 STR 20R. REMOVED DAMAGE AND REPAIRED PER SRM 53-30-3.SDR UPS99231123Battery Pack · bischargedINSPECTION TYPE: SI, RIGHT SIDE LOWER EXTERNAL EMERGENCY LIGHT OUT. VERIFIED WIRES AND LIGHT GOOD. REMOVED AND REPLACED BATTERY PACK AND PERFORMED FUNCTIONAL CHECK PER MM 33-50-101, MM 33-50-22.SDR UPS99231122Battery Pack · dischargedINSPECTION TYPE: SI, LEFT SIDE UPPER EXTERNAL EMERGENCY LIGHT OUT. VERIFIED WIRES AND LIGHTS GOOD PER WDM 33-51-01. REMOVED AND REPLACED EMERGENCY BATTERY PACK AND FUNCTIONALLY TESTED PER MM 33-50-101, MM 33-50-11, MM 33-50-81.SDR UPS99231098Seat Track · corrodedINSPECTION TYPE:SI, CORROSION ON SEAT TRACK AT BS 379, LBL 1, WL 208. REMOVED CORROSION ON SEAT TRACK, FOUND TO BE OUT OF LIMITS PER SRM 51-10-6 AND SRM 53-10-1. REMOVED CORRODED SEAT TRACK FROM BS 360 TO 545, BL 0 AND INSTALLED NEW SEAT TRACK PER SRM 51-30SDR UPS99231097Frame · corrodedINSPECTION TYPE:SI, CORROSION (C53-111-01.00-01) ON AFT E & E DOOR FRAME AFT SIDE AT BS 451. REMOVED FRAME AND REPLACED WITH NEW FRAME.SDR UPS99231110Skin · corrodedINSPECTION TYPE:SI, CORROSION ON INNER SURFACE OF BOOST PUMP CAVITY 7302 AT THE 3 O'CLOCK POSITION. REPAIRED PER ER NR 99-6318.SDR UPS99231109Frame · puncturedINSPECTION TYPE:SI, FWD CARGO BAY FRAME UPPER FLANGE PUNCTURED BS 680 LBL 23 WL 148.5. CUT OUT DAMAGED AREA 1 X 3 ON FRAME CROWN AT BS 680 LBL 23 WL 148.5, FABRICATED REPAIR DOUBLER, HEAT TREATED & INSTALLED ALL WORK ACCOMPLISHED IAW SRM 53-10-1, SRM 51-30-2,SDR UPS99231107Chord · crackedINSPECTION TYPE:SI WHILE WORKING NRC 010078 FUSE 157, 870 LOWER CHORD IS CRACKED LBL 10 WL 138 (870 BULKHEAD AIR COND BAY SIDE). CUT OUT DAMAGED SECTION OF CHORD AND REPAIRED PER SRM 51-40-4 BY SPLICING IN A NEW SECTION.SDR UPS99231105Skin · corrodedINSPECTION TYPE:SI, CORROSION ON INNER SURFACE OF BOOST PUMP CAVITY 7302 AT THE 6 O'CLOCK POSITION. REPAIRED PER ER 99-6318.SDR UPS99231104Seat Track · corrodedINSPECTION TYPE:SI CORROSION ON LOWER SURFACE OF SEAT TRACK BS 739 LBL 63 WL 208 REPLACED SEAT TRACK SEGMENT FROM BS 660 TO BS 740 LBL 65 PER 727 SRM 53-10-5 AND 51-30-2 ***CPCP***SDR UPS99231099Seat Track · corrodedINSPECTION TYPE:SI, SEAT TRACK CORRODED AT BS 740, RBL 45, WL 208. REMOVED, FABRICATED AND INSTALLED NEW SEAT TRACK FROM BS 660 TO 745, RBL 45, PER SRM 53-10-5 AND 51-30-2.SDR UPS99231069Floorbeam · corrodedINSPECTION TYPE:SI LOWER FLANGE OF BS 600 FLOORBEAM CORRODED BL 0-RBL 25 WL 200 CORROSION CLEAN UP BEYOND ACCEPTABLE LIMITS. REMOVED AND REPLACED LOWER CHORD LBL 18 TO RBL 31 PER ER 99-6268 AND SRM 53-10-1.SDR UPS99231108Seat Track · corrodedINSPECTION TYPE:SI, CORROSION ON SEAT TRACK AT BS 882, LBL 1, WL 208. CORROSION WAS FOUND TO BE OUT OF LIMITS AND REPLACED THE SEAT TRACK FROM BS 870 - BS 958, BL 0, WL 208, ON CUSTOMER ID 010795 PER SRM 51-30-2.SDR UPS99231063Skin · corrodedINSPECTION TYPE:SI CORROSION (C53-111-03.00-01) BULGE IN FUSELAGE SKIN BS 344, LBL 16, LWL 148 AND LEVELING COMPOUND SEPARATED FROM INTERIOR STRUCTURE HORIZ WALKWAY BEAM FROM BS 335-BS 351, LBL 16, WL 152. REMOVED DAMAGE AND REPAIRED PER SRM 53-30-3.SDR UPS99231103Frame · punctureINSPECTION TYPE:SI, FWD BAY FRAME UPPER FLANGE PUNCTURED BS 680 RBL 23 (BELOW RT FLOOR TO SIDEWALL SUPPORT NUTPLATE). REMOVED DAMAGE AND REPAIRED PER SRM.SDR UPS99231062Track · corrodedINSPECTION TYPE:SI CORROSION (C57-581-06.00-03) ON NR 4 FLAP TRACK UPPER SURFACE AT MOUNT PADS. REPLACED FLAP TRACK PER 727 MM.SDR UPS99231061Seat Track · corrodedINSPECTION TYPE:SI CORROSION ON SEAT TRACK AT BS 362 AND 369 RBL 45, WL 208 OUT OF LIMITS. REPLACED SEAT TRACK FROM BS 340 TO 390 PER SRM 53-10-5.SDR UPS99231054Battery Pack · discharged2 EXIT LIGHTS IN OVER HEAD INOP LEFT WING EMERGENCY LIGHT INOP. REMOVED AND REPLACED BATTERY PACK. OPS CHECK GOOD.SDR UPS99231060Seat Track · corrodedINSPECTION TYPE:SI CORROSION ON SEAT TRACK AT BS 940 RBL 45 WL 208. REPLACED SEAT TRACK SEGMENT FROM BS 870 TO 960 RBL 45 PER 727 SRM 51-30-5, 51-10-2 AND 51-30-2.SDR UPS99231044Floorbeam · corrodedINSPECTION TYPE:SI, CORROSION AROUND FASTENER HOLES BS 360, WL 208 LBL 6 AND RBL 11. REMOVED AND REPLACED FLOORBEAM UPPER CHORD.SDR UPS99231058Support · crackedINSPECTION TYPE:SI CRACKED, T/E UPPER PANEL SUPPORT L CHANNEL JUST ABOVE THE VERTICAL BULB, APPROX 1 FT FROM THE OB END OF THE I/B AILERON. REMOVED, FABRICATED, AND INSTALLED REPLACEMENT SUPPORT PER SRM 51-20-1.SDR UPS99231056Frame · dentedINSPECTION TYPE:SI AFT BAY FRAME DENTED BS 1030 LBL 25 WL 150. REMOVED DAMAGE AND REPAIRED PER SRM 51-40-3.SDR UPS99231055Shear Tie · damagedINSPECTION TYPE:SI WHILE WORKING CARD NR 010022 FOUND SHEAR TIE WITH 2 EA EXISTING HOLES WITH EXCESSIVE DIAMETER AT BS 344 ABOVE RT NOSE CHORD WL 156. REMOVED DAMAGED SHEAR TIE AND REPLACED WITH FABRICATED SHEAR TIE.SDR UPS99231059Carriage · corrodedINSPECTION TYPE:SI CORROSION ON NR 4 FLAP CARRIAGE SPINDLE FWD SHIM MATING SURFACE ORDERED AND RECEIVED NEW NR 4 FLAP CARRIAGE AND INSTALLED PER MM 27-51-03.SDR UPS99231023Floorbeam · corrodedINSPECTION TYPE:SI, FLOORBEAM IS EXFOLIATED BS 640, LBL 34-44, WL 208 CORROSION BLEND OUT BEYOND ALLOWABLE LIMITS. REMOVED AND REPLACED FLOORBEAM UPPER CHORD PER TRAMCO ER 99-6134.SDR UPS99231021Angle · corrodedINSPECTION TYPE:SI, INTERCOSTAL SUPPORT BRACKET CORRODED BS 1166 LBL 65 WL 208. REMOVED AND REPLACED BRACKET.SDR UPS99231042Link · crackedINSPECTION TYPE:SI, WHILE WORKING 870 FLOORBEAM REPAIR CUST CARD NR 997981 FOUND EXPANSION LINK TO BE CRACKED BS 870 RBL 25 WL 208. REMOVED CRACKED EXPANSION LINK, INSTALLED NEW LINK PER SRM 51-30-2.SDR UPS99231101Floorbeam · corrodedINSPECTION TYPE:SI, CORROSION (C53-224-01.00-01) FLOORBEAM TOP CHORD BS 680 RBL 51, WL 208. REMOVED AND REPLACED TOP CHORD PER SRM 53-10-1, SRM 53-10-8, OHM 20-41-02, SRM 51-30-2.SDR UPS99231036Fitting · corrodedINSPECTION TYPE:SI, WHILE WORKING CARD NR 998054 FOUND CORROSION ON I/B SIDE OF BOTH LUGS OF CENTER HINGE FITTING MOUNT OF NR 8 SPOILER. REMOVED DISCREPANT FITTING AND INSTALLED NEW FITTING.SDR UPS99231027Fitting · corodedINSPECTION TYPE:SI, WHILE WORKING CUSTOMER CARD 997840 FOUND NR 7 SPOILER ATTACH FITTING ON T/E HAS CORRODED ACTUATOR MOUNT HOLES. REMOVED DISCREPANT FITTING AND INSTALLED NEW FITTING.SDR UPS99231133Beam · corrosionINSPECTION TYPE:SI CORROSION ON UPPER FLANGE OF LONGITUDINAL BEAM BS 825 AND BS 845 LBL WL 208. REMOVED CORRODED UPPER FLANGE ON LONGITUDINAL BEAM. FABRICATED NEW UPPER BEAM AND INSTALL NEW REPLACEMENT PART AND SPLICE PER SRM 51-30-2, 51-30-.
Back to Boeing 727-25C