EVIDENCE OF SURFACE CORROSION FOUND ON CENTER LANDING GEAR RIGHT TRUNNION FITTING LOWER MATING SURFACE AREA. SURFACE CORROSION ON CENTER LANDING GEAR RIGHT HAND TRUNNION FITTING LOWER MATING SURFACE AREA REMOVED AS PER SRM 51-21-01 VOLUME II PAGE 27. ORIGINAL THICKNESS = 2.650", MATERIAL REMOVED = 0.011", MATERIAL REMAINING = 2.639" FOUND WITHIN LIMITS AS PER SRM 53-40-00 VOLUME I FIGURE 15. REPAIR CLASSIFIED AS MINOR AS PER GMM 6-2-100.