What was found
THE NR 2, 3 AND 13 LEADING EDGE SLATS HAVE LOCALIZED DELAMINATION ON THE LOWER SKIN OF THE TRAILING EDGE WEDGE. DELAMINATION REPAIRED TEMPORARILY WITH STRUCTURAL ADHESIVE INJECTION UNTIL PERMANENT REPAIR CAN BE ACCOMPLISHED AT THE NEXT HMV. AN NDT INSPECTION WAS ACCOMPLISHED ON 21 MAR 2006. PERMANENT REPAIR IS SCHEDULED FOR AUG 28, 2006. THE DELAMINATION OF THE TRAILING EDGE WEDGE IS A KNOWN PROBLEM. REFERENCE: 777 MM 57-43-99/801.