CRACK-LIKE INDICATION WAS LOCATED STARTING IN BEAD ARE GOING ACROSS FACE FOR 1-1/2 INCH LONG. LIQUID PENETRANT INSPECTION WAS THE METHOD SPECIFIED AND USED FOR THE NOT EXAMINATION.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
CRACK-LIKE INDICATION WAS LOCATED STARTING IN BEAD ARE GOING ACROSS FACE FOR 1-1/2 INCH LONG. LIQUID PENETRANT INSPECTION WAS THE METHOD SPECIFIED AND USED FOR THE NOT EXAMINATION.