What was found
DURING D-CHECK, FOUND CORROSION ON UPPER SURFACE OF LEFT RAM AIR PLENUM ABOVE SECONDARY HEAT EXCHANGER. REMOVED CORROSION AS PER SRM 51-10-6. REMOVED FASTENERS PER SRM 51-30-2. NDT CHECK LOSS MATERIAL .090. ALODINED AND PRIMED PER SRM 51-10-2. FABRICATED TWO EXTERNAL DOUBLER AS PER SRM 57-30-3 FIG 8 2024-T3 3.75 BY 13 INCH .080 AND INSTALLED FASTENERS.