What was found
FOUND AND REPAIRED CRACKS IN THE FUSELAGE SKIN AT THE FOLLOWING LOCATIONS. STA 418, STR 21L, 2 EACH. STA 370 - STA 385, STR 22L, 5 EACH. STA 400 BELOW STR 23L, 1 EACH. STA 420, STR 20L, 2 EACH. STA 385, STR 23L, 1 EACH. REPAIRED CORROSION AT FS 415, STR 23L. ALL 6 EACH REPAIRS MADE PER BOEING AIRCRAFT SRM 53-30-3, FIGURE 14.