What was found
NUMBER 3 SLAT HAS PITTING IN THE LEADING EDGE SKIN AT PREVIOUS BLEND SITES. REMOVED DAMAGED AREA AND INSTALLED FLUSH DOUBLER PER SRM 57-43-01-2.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
NUMBER 3 SLAT HAS PITTING IN THE LEADING EDGE SKIN AT PREVIOUS BLEND SITES. REMOVED DAMAGED AREA AND INSTALLED FLUSH DOUBLER PER SRM 57-43-01-2.