TUL - CORROSION ON FORWARD CARGO CHILL DUCT WEB BOTTOM SIDE OF CEILING, STA 775 TO STA 805 AT MINUS 25 OF CENTERLINE. REMOVED DAMAGED AREA, INSTALLED DOUBLER PER SRM 53-00-01. TST: 71,127.03 HOURS. CYCLES: 29,268. (X)