What was found
DURING LINE MAINTENANCE, FOUND CORROSION OF FUSELAGE SKIN AROUND THE LEFT STATIC PORT PLATE. REMOVED LEFT STATIC PORT PLATE, FOUND FUSELAGE SKIN UNDER THE PLATE CORRODED BEYOND LIMITS. REPAIRED SKIN IAW DC9 SRM 53-04, FIGURE 31, SHEET 1.