As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
What was found
LAV WASTE VACUUM OUTLET CUTOUT IS CORRODED. ACFT GROUNDED. REMOVED CORROSION ORIGINAL MATERIAL THICKNESS IS .071, REMOVED .002 WITH .069 REMAINING IS FOUND TO BE WITHIN LIMTIS IAW SRM 53-00-01-1A-1 ALLOWABLE DAMAGES 1 CHAPT 4-B-2-B, FIGURE 103, DETAIL C. APPLIED ALODINE AND PRIME IAW SRM 51-20-01. PRINTED AREA IAW AMM 51-21-99-300-801. REMOVED DOT.