What was found
FORWARD CARGO COMPARTMENT, LT TRANSITION PANEL CORRODED IN VARIOUS SPOTS BETWEEN FRAMES 500C-500F. GROUNDED - YES. REMOVED DAMAGE BETWEEN FRAMES 500C TO 500F AD CHECKED LIMITS ORIG THICKNESS .040 PER SRM 53-30-53-01-2. REMOVED .011 REMAINING .029 FOUND TO BE OUT OF LIMITS PER SRM 53-00-53-1A-2, REMOVED FACTORY SPLICE PLATE PER SRM 51-40-02, REMOVED DAMAGED SECTIONS BETWEEN STA 500B +9 TO 500C + 15 AND 500D-5 TO 500F+9 PER SRM 53-00-53-2R-5, FABRICATED REPAIR PARTS PER SRM 53-00-53-2R-5, ALODINED AND PRIMED PARTS PER SRM 51-20-01 AND SOPM 20-42-02, INSTALLED REPAIR FROM STA 500B +9 TO 500C +15 AND 500D -5 TO 500F +9 PER SRM 53-00-53-2R-5, REINSTALLED FACTORY SPLICE PLATE AT STA 500D-6 PER SRM 51-40-01.