What was found
FWD CARGO LT TRANSITION PANEL STA 500G+2 TO 500I HAS CORROSION. GROUNDED - YES. REMOVED CORROSION FROM THE FWD PIT L/H TRANSITION PANEL AT STA 500G+2 TO 500I IAW B737-800 SRM 53-00-53-1A-2.2.D ORIG THICKNESS IS .040 IAW B737-800 SRM 53-30-53-01-2 TABLE 2. REMOVED .008. REMAINING THICKNESS IS .032 AND IS FOUND TO BE OUT OF LIMITS PER. B737-800 SRM 53-00-53-1A-2.4.A.(2). REPAIRED THE FWD PIT L/H TRANSITION PANEL FROM STA 500F+10 TO 500I WITH BAC 1496-444 PO: 1088630.1 PER. B737-800 SRM 53-00-53-2R-5 REMOVE DOT.