What was found
GSO - INSPECTION FOUND A .50 INCH CRACK IN FRAME TO STRINGER ATTACH ANGLE AT STR 26R, STA 333. THE CRACKED ANGLE WAS REMOVED AND A NEW ANGLE WAS FABRICATED AND INSTALLED IAW SRM 51-10-2, SRM 51-30-2, AND SRM 53-10-3. (X)
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
GSO - INSPECTION FOUND A .50 INCH CRACK IN FRAME TO STRINGER ATTACH ANGLE AT STR 26R, STA 333. THE CRACKED ANGLE WAS REMOVED AND A NEW ANGLE WAS FABRICATED AND INSTALLED IAW SRM 51-10-2, SRM 51-30-2, AND SRM 53-10-3. (X)