What was found
INSPECTION FOUND A 2 INCH CRACK IN RT VERTICAL STABILIZER BANANA FAIRING. THE CRACKED AREA WAS REMOVED AND A FILLER AND DOUBLER WERE INSTALLED IAW SRM 55-01, FIGURE 2 AND 55-03, FIGURE 17.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
INSPECTION FOUND A 2 INCH CRACK IN RT VERTICAL STABILIZER BANANA FAIRING. THE CRACKED AREA WAS REMOVED AND A FILLER AND DOUBLER WERE INSTALLED IAW SRM 55-01, FIGURE 2 AND 55-03, FIGURE 17.