As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
What was found
WHILE ACCOMPLISHING EQ3412 FOUND LEFT SIDE LOWER ATTACHMENT AREA OF WINDSHIELD SIDE POST GOUGED ON TOP SIDE OF AREA. BLENDED GOUGE REF SRM 51- 73-00. BLENDED AREA AFTER REWORK IS 1.75"X1.25"X.020" DEEP. ORIGINAL MATERIAL THICKNESS AT AREA IS .600". PER FIG 1, PAGE 8 WITHIN SERVICEABLE LIMITS, WILL NEED HFEC & PAINT RESTORED.