LH HORIZONTAL STAB LOWER SKIN HAS 2 CRACKS. CRACK 1- STA 138.70 L= .500". CRACK 2 - STA 120.30 = .400". 01 AMM 51-21-73-370-801, AMM 51-21-00-100-801, PERFORMED NDT IAW PART 6, 51-00-00 PROC 16 PROC 23, HFEC NDT INSPECTION ACCOMPLISHED ON ALL 3 CUTOUTS AND ALL OUTER FASTENER HOLES DIP PER ABOVE REQUIREMENTS. REMOVED PREVIOUS REPAIR AT STA 120-136 IAW SRM 55-10-01 REP 11 TABLE 204.