What was found
THREE SCRATCHES ON RT PRIMARY STATIC PORT (A-73). BLENDED AND EVALUATED SCRATCHES ON THE RT PRIMARY STATIC PORT, BLEND NR 1 LOCATED BTW BS 417 AND 4" ABOVE OF THE S16R ORIGINAL THICKNESS: 0.080" MATERIAL LOSS: 0.002" MATERIA L REMAINING: 0.078", BLEND NR 2 BTW STA 414 AND .500" ABOVE OF S16R ORIGINAL THICKNESS: 0.080" MATERIAL LOSS: 0.002" MATER IAL REMAINING: 0.078", BLEND NR 3 BTW BS 408 AND 4" ABOVE OF S16R ORIGINAL THICKNESS: 0.080" MATERIAL LOSS: 0.002" MATERIAL REMAINING: 0.078", FOUND TO BE WITHIN LIMITS, PERFORMED NDT NO CRACKS NOTED, APPLIED ALODINE, MEASURED THE SKIN WAVINES FOUND TO BE WITHIN LIM ITS IAW SRM 53-30-01-1A-2, 51-10-02-0G-0, 51-20-01-0G- 0, 51-10-01-0G-0, AMM 34-11-02-200-802.