What was found
INSPECTION FOUND LOWER CAP OF FLOORBEAM CORRODED AT FS 1070 FROM LBL 39 TO RBL 48. THE LOWER CAP WAS CUT OUT, L-ANGLES, FILLER AND A STRAP WERE FABRICATED AND INSTALLED IAW SRM 53-10-8, FIGURE 8.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
INSPECTION FOUND LOWER CAP OF FLOORBEAM CORRODED AT FS 1070 FROM LBL 39 TO RBL 48. THE LOWER CAP WAS CUT OUT, L-ANGLES, FILLER AND A STRAP WERE FABRICATED AND INSTALLED IAW SRM 53-10-8, FIGURE 8.