What was found
RIGHT WING NR 10 L/E SLAT UPPER O/B SURFACE DELAMINATED. METAL HOT BOND REPAIR CARRIED OUT AS PER SRM 57-43-02 REPAIR 1 AND SRM 51-70-10 REPAIR 4, SHEET 2.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
RIGHT WING NR 10 L/E SLAT UPPER O/B SURFACE DELAMINATED. METAL HOT BOND REPAIR CARRIED OUT AS PER SRM 57-43-02 REPAIR 1 AND SRM 51-70-10 REPAIR 4, SHEET 2.