What was found
INITIAL: EXFOLIATION CORROSION ON INTERNAL FUSELAGE SKIN BETWEEN STA Y= 230 TO 237 AND LONG 25 RT TO 26 RT AT FWD CARGO COMPARTMENT. FINGER DOUBLER WAS CUT FOR EXCESSIVE DAMAGE AND NEW DOUBLER WAS FABRICATED IAW SRM 53-04, FIG 12D AND SKIN CORROSION WAS REMOVED IAW SRM 51-10-3, PAR 26, 21, 14.