What was found
HIDDEN CORROSION: CORROSION LOWER JAMB AT AFT CARGO COMPARTMENT BELOW SCUFF PLATE AREA. SUMMARY OF NRC 00199 CORROSION LEVEL I, CORROSION ON LOWER JAMB WAS REMOVED PER MD-90 VOL.II SRM 51-10-03 PAR.26 (UT) WAS ACCOMPLISHED PER NDT 04-00-07 PAR.5 FIG.3 SHEET 1&2 ORIGINAL THICKNESS ON LOWER JAMB IS 0.160" AND MINIMUM REMAINING THICKNESS IS 0.145" . THEREFORE IT IS WITHIN LIMITS PER MD-90 VOL.I SRM 53-60-02 PAR.11 FIG.9 (SHEET 2). (LP# 0828103)