What was found
CORROSION WAS FOUND ON THE LH FLAP INBOARD HINGE FITTING FASTENER HOLES (8 ATTACH POINT) IN REF NRC 258. SUMMARY OF NRC 00861: LEVEL CORROSION 2. LH FLAP INBOARD HINGE FITTING WAS REPLACED PER B717 AMM 57-55-25. (LP #0528717)
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
CORROSION WAS FOUND ON THE LH FLAP INBOARD HINGE FITTING FASTENER HOLES (8 ATTACH POINT) IN REF NRC 258. SUMMARY OF NRC 00861: LEVEL CORROSION 2. LH FLAP INBOARD HINGE FITTING WAS REPLACED PER B717 AMM 57-55-25. (LP #0528717)