What was found
AFTER WASTE PANEL REMOVAL CORROSION WAS FOUND ON FUSELAGE SKIN 1680 TO STA 1700 AND S25R TO S28R AT LOWER FUSELAGE. CORROSION LEVEL 2: FUSELAGE SKIN 1680 TO STA 1700 AND S25R TO S28R AT LOWER FUSELAGE WAS REPAIRED PER PRI 633487-14 REV 0, PRI 633487-14 REV 1, PRI 633487-14 REV 2, PRI 633487-14 REV 3 AND ER/A 633487-14AD REV. ORIGINAL. (1544656)