What was found
RT WING INBD VANE SLOT UPPER SKIN CORRODED AT STA XILD 0.7095. (MAJOR REPAIR) PERFORMED MAJOR REPAIR. REMOVED FASTENERS. REMOVED CORROSION. FOUND OUT OF LIMITS. TRIMMED OUT AND REMOVED DAMAGED AREA. PERFORMED NDT INSPECTION IAW NDT STANDARD PRACTICE MANUAL PART 6-10-01-001. FABRICATED FILLER AND DOUBLER IAW ASTAR ED EDU21-11, ASTAR DWG U21-R11. CLEANED, TREATED AND PRIMED AREA AND FILLER AND DOUBLER INTERNAL PART IAW SRM 51-1-8B. APPLIED PRC SEALANT ON FAYING SURFACES IAW SRM 51-1-11 PG 9. INSTALLED FILLER AND DOUBLER WITH NEW FASTENERS IAW ASTAR ED EDU21-11, ASTAR DWG U21-R11, SRM 51-1-20D PG 9, SRM 51-1-21 PG 1.