What was found
RT OUTER WING INBD EXTENDED L/E OUTER PLATING SHOWS CORROSION & ELONGATED HOLES AROUND STA XFS 710 (MAJOR REPAIR). PERFORMED MAJOR REPAIR. REMOVED FASTENERS, REMOVED CORROSION, FOUND OUT OF LIMITS. TRIMMED OUT THE CORRODED SKIN AREA. PERFORMED NDT INSPECTION. CLEANED, TREATED AND PRIMED AREA, FABRICATED A REPAIR DOUBLER A FILLER AND A TRIPLER. CLEANED, TREATED AND PRIMED DOUBLER AND TRIPLER INTERIOR SURFACE AND FILLER. APPLIED PRC SEALANT ON FAYING SURFACE AND FILLER. INSTALLED FILLER AND DOUBLER AND TRIPLER ON RT OUTER WING INBD EXTEDNED L/E OUTER PLATING (AROUND STA XFS 710.000) USING NEW FASTENERS.