What was found
SURFACE CORROSION ON STRINGER 30 FROM BS 1150 TO 1166. REMOVED CORROSION IAW SRM 51-10-6. AREA FOUND WITH IN LIMITS IAW SRM 53-10-1 FIGURE 1 AND 53-10-2 FIGURE 9. FOUND CORROSION BETWEEN BS 1150-1155 TO BE OUT OF LIMITS IAW SRM 53-10-1 FIGURE 1 AND 53-10-2 FIGURE 9. CUT OUT DAMAGED SECTION OF STRINGER IAW SRM 53-10-3 FIGURE 1. FABRICATED FILLER STRINGER AND 2 EACH SPLICE STRINGER IAW SRM 53-10-3 FIGURE 1. TREATED AND PRIMED PART AND AREA IAW SRM 51-10-2. INSTALLED REPAIR PARTS IAW SRM 53-10-3 FIGURE 1.