What was found
DURING CORROSION VISIT INSPECTION, CORROSION WAS FOUND ON THE FUSELAGE SKIN AT STA 1010, BETWEEN STRINGER 29L AND STRINGER 30. A 2.5 BY 2.5 CUTOUT IN THE SKIN WAS REQUIRED, STRINGER 30 WAS CUT AFT OF THE FACTORY SPLICE. BOTH DAMAGE LOCATIONS WILL BE REPAIRED IN ACCORDANCE WITH B727 SRM 53-10-3 FIG 1 FOR THE STR AND B727 SRM 53-30-3 FIG 3A, FOR THE SKIN.