What was found
DURING CORROSION INSPECTION, RIGHT WING NR 6 SLAT WAS FOUND WITH A .5 INCH CRACK IN O/B ATTACH ANGLE, JUST I/B OF O/B STOP. REPAIRED PER MM 57-54-0 PG 816.