CORROSION WAS FOUND IN STRINGER 39L AT STATION 1540 AND WAS BEYOND ALLOWABLE LIMITS. A REPLACEMENT SECTION OF STRINGER WAS SPLICED IN PER SRM 53-00-03-2-202.