What was found
DURING HMV-2, CORROSION DAMAGE WAS FOUND ON THE C2 & C3 JAMB BEAMS. THE JAMB BEAM DOOR STOP HOLES WERE OUT OF TOLERANCE AFTER CLEAN UP. CORROSION WAS REPAIRED PER MD80 SRM 53-05 FIGURE 63 BY BLENDING AND USE OF A REPAIR DOUBLER.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
DURING HMV-2, CORROSION DAMAGE WAS FOUND ON THE C2 & C3 JAMB BEAMS. THE JAMB BEAM DOOR STOP HOLES WERE OUT OF TOLERANCE AFTER CLEAN UP. CORROSION WAS REPAIRED PER MD80 SRM 53-05 FIGURE 63 BY BLENDING AND USE OF A REPAIR DOUBLER.