What was found
EROSION AND DELAMINATION ON LOWER SURFACE DENTS ON UPPER SURFACE OF LT INNER FLAP OUTBD VANE. DOUBLER, FILLER REPAIR BONDING WAS DONE IAW SRM 51-70-2D PARA H. REPAIRED IAW SRM 57-03D PARA 8A FIG 9A.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.