DURING HMV AT GDL, CORROSION WAS FOUND IN THE AFT CARGO COMPARTMENT INTERNAL DOOR JAMB DOUBLER AT STA 1209 BETWEEN S-29R AND S-30R. THE DAMAGE WAS REPAIRED PER BOEING INSTRUCTIONS.