What was found
LEFT FUSELAGE SKIN AREA OF SURFACE FINISH DETERIORATED AROUND FASTENER HEAD FR21/ STR 41. REPAIR CARRIED OUT IAW SRM 53-10-12, FIG 225, SH3, SRI 53-10-12-2-005-00 TABLE TO BE EMBODIED. INITIAL AT 42500FC OR89000FH, SUBSEQUENT AT TO BE DECIDED. INSP METHOD = ULTRASONIC/ EDDY CURRENT STRUCTURAL MODIFICATION POINT TO BE DECIDED.