What was found
MAIN DECK - LOWER OF LAVATORY UNIT BETWEEN FRAME 11 TO FRAME 12A AT FLOOR SUPPORT, CORROSION. REMOVED AS PER SRM 51-74-10 REV 75. MATERIAL REMOVED 0.061", MATERIAL REMAINED 0.017", MATERIAL THICKNESS 0.078" AND FOUND OUT OF LIMIT AS PER SRM 53-12-15 FIG 101 REV 75. DAMAGED FLOOR SUPPORT REMOVED AND REPLACED AS PER SRM 51-40-21 REV 75. REPAIR CLASSIFIED AS MINOR PER GMM 6-2-100 REV 112.