What was found
WATER TRAPPED IN LT RUDDER. THE OUTER SKIN CUT OUT 4.8" AND DRY THE AREA IAW SRM 55-41-12 STEP 1. PERFORMED A TAP-TEST FOR DAMAGE FREE IAW SRM 55-41-12, STEP 1. INSTALLED INNER SKIN WITH RESIN IAW SRM 51-77-10, PARA 2H. INSTALLED REPLACEMENT CORE AND FILLED GAPS AT CORE EDGES, CURE THE FILLER AT 149 DEGREES IAW SRM 55-41-12, STEP 2. PERFORMED OUTER SKIN REPAIR AND CURE THE RESIN AT 140 DEGREES IAW SRM 55-41-12, FIG 221 TRACKING IN SRM AND IAW IIR 55-41-12-2-006-00. REPAIR WAS CLASSIFIED AS MAJOR IAW GMM 6-2-100