What was found
HIGH FREQUENCY EDDY CURRENT INSPECTION CARRIED OUT ON LEFT HAND NOSE LANDING GEAR TRUNNION FITTING, STATION Y = 595 AND FOUND 01 EACH CRACK PROPAGATE FROM THE SLOT OUT AREA APPROXIMATE 1/4 INCHES LENGTH. 01 EACH PROPAGATED CRACK FROM THE SLOT OUT AREA AT LEFT HAND NOSE LANDING GEAR TRUNNION FITTING STATION Y = 595 REPAIRED AS PER SRM 53-10-14-2R REPAIR 2 FIGURE 202. INITIAL INSPECTION TO BE CARRIED OUT AT 1500 FLIGHT CYCLES AND REPETITIVE INSPECTION TO BE CARRIED OUT EVERY 1500 FLIGHT CYCLES PER SRM 53-10-14-2R TABLE 201 FIGURE 202 REPAIR 2 REQUIREMENTS. METHOD BY HIGH FREQUENCY EDDY CURRENT OR LIQUID PENETRANT. REPAIR CLASSIFIED AS MAJOR PER GMM 6-2-100.