What was found
RH INBOARD FLAP - DAMAGE / EROSION ON OUTBOARD TRAILING EDGE (REPAIR). REMOVE DAMAGE AREA AND SURFACE MOISTURE AND CLEAN THE DAMAGED AREA I.A.W. 747-8F SRM 57-53-01-2R-1 REFER TO SRM 51-70-04-2R-1 PARAGRAPH 5.A.(1), (2) REV.43. REMOVE THE DAMAGE AND TAPER SAND. RECORD THE DAMAGE AREA (LENGTH:0.5", WIDTH:0.4", 9" FROM TRAILING EDGE, 19" FROM OUTBOARD EDGE) I.A.W. 747-8F SRM 57-53-01-2R-1 REFER TO SRM 51-70-04-2R-1 PARAGRAPH 5.A.(3), (4) REV.43. REMOVE FLUIDS, AND OTHER CONTAMINATION HEAT AREA TO 150°F TO 170°F HOLD FOR 8 HOURS MINIMUM I.A.W. 747-8F SRM 51-70-04-2R-1 PARAGRAPH 5.A.(5). REFER TO SRM 51-20-15-2R-1 REV.43. BOND THE REPAIR PLIES WITH RESIN AND CURE AT 200°F FOR 240 MINUTES WITH MINIMUM VACUUM OF 22 IN/HG I.A.W. 747-8F SRM 51-70-04-2R-1 PARAGRAPH 5.A.(7). THRU PARAGRAPH 5.D REV43. PAPER FINAL REVIEW OK