As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
What was found
FLOOR BEAM STA 560 BTWN BL-0 AND LBL 24.75 IS CORRODED. DOT 142-326. EVALUATED DAMAGE IN FLOOR BEAM STA 560 BTWN BL-0 AND LBL24.75.:P1)ORIGINAL THICKNISS 0.220'' MATERIAL LOSS 0.010'' MAXIMUN ALLOWABLE 0.022'' MATERIAL REMANING 0.210''.P2) ORIGINAL THICKNISS 0.220'' MATERIAL LOSS 0.008'' MAXIMUN ALLOWABLE 0.022'' MATERIAL REMANING 0.212''FOUND WITHIN LIMITS .IAW SRM 53-00-51-1A-1.