What was found
MDC FR75-77, Y1580.5 TO Y2127.5, Z ANGLE ON A CORNER OF FLOOR STR AREA, THERE IS A CRACK.REMOVED Z-PROFILE FROM MDC FR75 TO FR77 WITH CRACK IAW A300-600 SRM 51-40-21. FABRICATED Z-PROFILE USING MATERIAL 5052-H34.071, BATCH 0004399222, IAW GMM 09-08 PARAGRAPH 09.08.01.04 AND SRM 53-18-18, FIGURE 3 (SHEET 2), ITEM 50.INSTALLED NEW Z-PROFILE ON MCD BETWEEN FR 75 TO FR 77 L/H SIDE USING FASTENERS 35(EA) P/N MS20426AD5-7, BATCH 0004372118 IAW SRM 51-40-21 AND SRM 51-76-10