What was found
CRACKED WEDGE, RT WING OUTBD FLAP INBD WEDGE. REMOVE THE CRACK MATERIALS AND CLEAN. BOND THE REPAIR PLIES WITH RESIN CURED AT 200°F FOR 220 MINUTES WITH MINIMUM VACUUM OF 22 IN/HG. I.A.W UPS SREO-70175-REQ001 REV.1
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
CRACKED WEDGE, RT WING OUTBD FLAP INBD WEDGE. REMOVE THE CRACK MATERIALS AND CLEAN. BOND THE REPAIR PLIES WITH RESIN CURED AT 200°F FOR 220 MINUTES WITH MINIMUM VACUUM OF 22 IN/HG. I.A.W UPS SREO-70175-REQ001 REV.1