DURING C CHECK INSPECTION, LT FUSELAGE NOSE SECTION LWR PLATING UPPER AFT CORNER BROKEN OFF AT BS 70 L-33. PERFORMED MAJOR REPAIR IAW DC8 SRM 53-2-2 FIG 8C-2, TR NR 53-176, EO SEMAN NR 20051299 DATED 09-29-05. PERFORMED DETAIL VISUAL INSPECT. NEITHER CRACK NOR CORROSION FOUND. FABRICATED REPAIR DOUBLER IAW DC8 SRM 53-2-5 FIG 8C-2, DC8 SRM 53-2-5 FIG 8B-2, DC8 SRM 53-3-1 FIG 1 ITEM A, DC 8 SRM 53-4-1 FIG 1 ITEM C, DC8 SRM 51-9-0 FIG 68A. INSTALLED REPAIR DOUBLER IAW DC8 SRM 53-2-5 FIG 8C-2, DC8 SRM 51-1-20D, DC8 SRM 51-3-1.