What was found
DURING C CHECK, 2 CORRODED AREAS FOUND ON LOWER FUSELAGE NOSE SECTION AT FOLLOWING LOCATION BS 217 BETWEEN L32 & 31R, BS 223 BETWEEN L32R & 32L, DUE CHANGE. PERFORMED REPAIR IAW DC-8 SRM 53-2-1. REMOVED CORROSION IAW DC8 SRM 51-1-8, FOUND OUT OF LIMITS IAW DC8 SRM 53-2-0. REMOVED CORRODED PLATING SEGMENT. CUT OUT DAMAGED SECTION. FAB`D EXTERNAL SPLICES, INTERNAL FINGER DOUBLER, INTERNAL DOUBLER, TR NR 53-173 DATED 09-20-03. CLEANED, TREATED & PRIMED AREA, REPAIR PART. APPLIED SEALANT TO FAYING SURFACES. INSTALLED NEW PLATING SEGMENT & REPAIR PART. ALL WORK PERFORMED IAW APPLICABLE SRMS.