What was found
DURING C18 CHECK INSPECTION, FOUND A CRACK AT STRINGER S25L END, BS 676, POINTING AFT. DAMAGE IS LOCATED AT THE STRINGER WEB EXTENDING FOR ABOUT 5 INCHES. TRIMMED OUT DAMAGED. PERFORMED HFEC INSPECTION OF TRIM OUT AND 3 INCHES AROUND INSURE CRACK FREE IAW NDT PART 6. TOUCHED UP EXPOSED EDGE OF STRINGER TRIM OUT AND ANY BARE AREA OF THE SURROUNDING STRUCTURE WITH CHEMICAL CONVERSION COATING IAW SRM 51-20-01. INSTALLED REPAIR PARTS AS SHOWN IN FIG 3 OF REPAIR EA MF00852R0006.