DURING ROUTINE INSPECTION CRACKS ON THE HINGE SURFACE RADIATE FROM MOUNTING BORES. THIS IS A VERY COMMON FAILURE FOR THIS PART. SUGGEST PART BE MANUFACTURED FROM A MORE DURABLE MATERIAL SUCH AS STAINLESS STEEL OR TITANIUM. (K)