LEVEL 1 CORROSION APU BATTERY COMPARTMENT DOOR INNER SURFACE. REMOVED CORROSION PER BOEING SRM 51-10-01 WITHIN LIMITS PER 52-00-02, TREATED PER 51-10-02.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
LEVEL 1 CORROSION APU BATTERY COMPARTMENT DOOR INNER SURFACE. REMOVED CORROSION PER BOEING SRM 51-10-01 WITHIN LIMITS PER 52-00-02, TREATED PER 51-10-02.