LEVEL 1 CORROSION MAIN DECK BS 800 FLOOR BEAM RIGHT END REINFORCING PLATE IN BOTH UPPER AND LOWER SURFACE. REMOVED CORROSION AND REPROTECTED AREA PER BOEING 51-10-01 AND 51-10-02.