FLOOR SUPPORTS AT FR80 STR29L-29R CORRODED. BLENDED OUT FLOOR SUPPORT AT FR 80 STR 29L-29R ORIGINAL THICKNESS 0.063" MAT LOSS 0.003" REMAINING THICKNESS 0.060" FOUND TO BE IN LIMITS IAW SRM 53-23-04.