What was found
DURING A SCHEDULED INSPECTION, 3 AREAS OF THE PRIMARY FUSELAGE SKIN HAD CORROSION DAMAGE THAT WAS COMPLETELY THROUGH THE SKIN THICKNESS. DAMAGE AREA WAS APPROX 1 SQ INCH AT EACH DAMAGE LOCATION. THE AREAS WERE LOCATED AT; 1 EA AREA UNDER THE REFUELING GROUND CLIP LT FUSELAGE SKIN AT STA 5100MM, WL 1600MM. 2 EA AREAS; ONE ON BOTH LT AND RT FUSELAGE SKINS AT THE AFT ENGINE COWLING LATCH PLATE. FUSELAGE STA 5800, WL2600MM. (K)